Every year, millions of tons of PVC window and door profiles reach end-of-life. These profiles contain not only high-quality PVC resin but also valuable embedded materials: aluminum hardware, galvanized steel reinforcements, stainless steel fasteners, glass fragments, and EPDM rubber gaskets.
Without proper separation technology, this mixed waste is either landfilled or downcycled into low-value products.
The Core Challenge
The difficulty lies in the complete liberation of embedded materials. Steel reinforcements are wrapped inside PVC. Glass fragments are mixed with rubber particles. Aluminum hardware is scattered throughout.
Our solution: one separation principle per stage, combined into a complete process route.
Process Flow
Pre-Treatment & Shredding
Remove large hardware and extract glass panels intact. The single shaft shredder cuts profiles into small segments — glass shatters while PVC remains in chunks, initiating natural liberation.Output: ≤80–100 mm
First Glass Removal
Overband magnet removes liberated ferrous metals. Linear Screen ① (10–15 mm) separates glass from PVC chunks — removing 70–85% of bulk glass.
Hammer Mill Liberation
Hammer mill breaks steel, aluminum, and residual glass free from PVC matrix. Moving hammer heads withstand metal impact — the only choice for dirty material.
Industrial Metal Crusher Hammer Crusher Machine
Second Glass Removal & Metal Cleanup
Linear Screen ② (5 mm) captures fine glass dust before pulverizer. Magnetic roller removes residual ferrous and weakly magnetic stainless steel — protecting the eddy current rotor.
Eddy Current Separation
Eddy current separator recovers aluminum at the optimal 5–20 mm feed size. Eccentric rotor ejects fine aluminum cleanly without material wrapping.
Final Protection & Pulverizing
Metal detector ejects remaining metal before pulverizer — one set of grinding discs costs far more than this detector. Water-cooled pulverizer grinds PVC to 20–30 mesh powder. Rubber flattens but stays at millimeter scale, creating size differential for screening.
Bulk removal after shredding → fine dust capture after hammer milling → tolerate sub-75 μm residual (ash <1%). Glass cullet is sellable — the earlier it’s removed, the more valuable.
2. Hammer Mill for Dirty Material
Moving hammers withstand metal impact. Clean material can use crusher for better shape and lower energy.
3. Four-Stage Metal Protection
Overband Magnet → Magnetic Roller → Eddy Current → Metal Detector. Progressive cleanup protects the pulverizer grinding discs.
Quality Control
Ash
Application
<1%
Light-colored products
1–3%
Dark-colored products
Batch-to-batch consistency matters more than absolute values. Stable ash content allows customers to keep extrusion parameters unchanged when blending 10–30% recycled powder.