Every golf ball manufacturer faces a common problem: rejected, cured cores that cannot be sold. These cores consist primarily of vulcanized polybutadiene rubber (BR)—a material that is notoriously difficult to grind due to its elasticity, heat sensitivity, and tendency to smear rather than fracture. The situation is further complicated by 15–20% plastic contamination from thermoplastic covers, ionomer layers, and paint coatings. At ambient temperatures, this composite material deforms under mechanical stress, generates excessive heat during grinding, and re-agglomerates into unusable clumps.
Our Solution: Two-Stage Low-Temperature Process
WANROOETECH has developed a proven two-stage process specifically for elastic rubber materials like golf ball cores. The system combines controlled-temperature coarse crushing with precision fine grinding, available in both cryogenic and mechanical cooling configurations. This approach ensures consistent particle size distribution, prevents thermal degradation, and maximizes rubber recovery rates.
Stage 1: PNSC Series Strong Crusher
The PNSC crusher serves as the critical first step, reducing whole golf ball cores to 8–15 mm particles without the smearing and heat buildup typical of conventional shredders. Key design features include:
Tangential feed design: Prevents elastic rubber from bouncing back or bridging in the hopper
Claw-type blades: High-carbon tool steel (SKD-11) construction resists impact and abrasion; resharpenable for extended service life
Different production goals require different cooling approaches. We offer both configurations on the same PNMF platform.
Option A: Cryogenic Grinding (Liquid Nitrogen) Uses liquid nitrogen to cool rubber below its glass transition temperature (approximately -196°C), causing vulcanized BR to become brittle and fracture cleanly. This method delivers superior powder quality with smooth particle surfaces and narrow size distribution, making it ideal for premium applications requiring 250 μm fine powder.
Option B: Mechanical Cooling (Water + Forced Air) The PNMF’s standard dual cooling system maintains safe operating temperatures without liquid nitrogen. An optional industrial chiller further reduces chamber temperature for enhanced performance. This approach offers lower operating costs (approximately 120–180 kWh per ton) and is well-suited for 500 μm target sizes.
EN: We recognize that vulcanized polybutadiene with thermoplastic contamination presents unique processing challenges. That’s why we offer comprehensive testing services:
Laboratory trials: Send 50–100 kg of your material for testing on our PNLP laboratory pulverizer. Receive complete data on particle size distribution, energy consumption, and separation efficiency.
Industrial pilot runs: For larger validation batches, schedule time on our PNMF-500 production unit.
Process optimization: Based on trial results, we adjust blade geometry, disc gap, and cooling intensity to meet your specific requirements—with written performance guarantees.